| Grade : | X46Cr13 |
| Number: | 1.4034 |
| Standard: | EN 10088 - 2 : 2005 Stainless steels. Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes EN 10088 - 3 : 2005 Stainless steels. Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes |
| Classification: | Martensitic stainless steels - standard grade |
| Equivalent grades: | Go here |
| Tighter carbon ranges may be agreed at the time of enquery and order Particular ranges of sulphur content may provide improvement of particular properties. For machinability a controlled sulphur content of 0.015 % to 0.030% is recommended and permitted. For weldability, a controlled sulphur content of 0.008 % to 0.030 % is recommended and permitted. For polishability, a controlled sulphur content of 0.015 % max is recommended. Elements not listed in this table shall not be intentionally added to the steel without the agreement of the purchaser except for finishing the cast. |
| C | Si | Mn | P | S | Cr |
| 0.43 - 0.5 | max 1 | max 1 | max 0.04 | max 0.015 | 12.5 - 14.5 |
| Poland PN | Russia GOST | ||
|
|
| ReH | Minimum yield strength / Mindestwert der oberen Streckgrenze / Limite d’elasticite minimale |
| Rm | Tensile strength / Zugfestigkeit / Resistance a la traction |
| A | Minimum elongation / Mindestwert der Bruchdehnung / Allongement minimal |
| J | Notch impact test / Kerbschlagbiegeversuch / Essai de flexion par choc |